[ASAP] Trickle Flow Aided Atomic Layer Deposition (ALD) Strategy for Ultrathin Molybdenum Disulfide (MoS<sub>2</sub>) Synthesis ACS Applied Materials & InterfacesDOI: 10.1021/acsami.9b12023 Published in: "Applied Materials and Interfaces".admin2019-09-20T20:40:21+00:00September 20th, 2019|Categories: Publications|Tags: MoS2| Share This Story, Choose Your Platform! FacebookTwitterLinkedInEmail Related Posts